Výsledky vyhľadávania
- Description of defects by type for six grades of red oak lumber.
Harding O.v.
Steele P.h.
Kamarul Za Man Nordin
For. Prod. J.. Roč. 43, č. 6 (1993), s. 45-50
xcla - ČLÁNKY - Relative kerf and sawing variation values for some hardwood sawing machines.
Steele P.h.
Wade M.w.
Bullard S.h.
Araman Philip A.
For. Prod. J.. Roč. 42, č. 2 (1992), s. 33-39
xcla - ČLÁNKY - Influence of softwood sawmill size on lumber recovery.
Steele P.h.
Wagner F. G.
Lin Y.n.
Skog Kenneth E.
For.Prod.J.. Roč. 41, č. 4 (1991), 68-73, 5 tab., res. angl., lit.12.
xcla - ČLÁNKY - The stope-of-grain indicator for defect detection in unplaned hardwood lumber.
Steele P.h.
For.Prod.J.. Roč. 41, č. 1 (1991), s. 15-20
xcla - ČLÁNKY - Moisture content variation of lumber processed at roughmills.
Steele P.h.
For.Prod.J.. Roč. 40, č. 11/12 (1990), s. 19-24
xcla - ČLÁNKY