- Theoretical basis of fractographic methods and their application in f…
Počet záznamov: 1  

Theoretical basis of fractographic methods and their application in fracture modelling for Cr-Ni steels

  1. NázovTheoretical basis of fractographic methods and their application in fracture modelling for Cr-Ni steels
    Aut.údajeVeronika Klopanová ... [et al.]
    Autor Nováková Veronika 1992- (25%) UMBFP10 - Katedra matematiky
    Spoluautori Novák Viktor 1982- (25%)
    Kvasnová Petra 1978- (25%) UMBFP07 - Katedra techniky a technológií
    Novák Daniel 1952- (25%) UMBFP07 - Katedra techniky a technológií
    Zdroj.dok. Manufacturing Technology : Journal for Science, Research and Production. Vol. 17, no. 6 (2017), pp. 869-876. - Ústí nad Labem : Univerzita Jana Evangelisty Purkyně v Ústí nad Labem, 2017
    Kľúč.slová fraktografia - fractography   optická mikroskopia - svetelná mikroskopia - optical microscopy   Cr-Ni oceľ  
    Jazyk dok.angličtina
    KrajinaČeská republika
    Systematika 62
    AnotáciaFraktografické metódy čerpajú svoje poznatky z euklidovskej geometrie, teórie množín, teórie miery a teórie chaosu. V strojárskej technológii sa fraktografia používa predovšetkým na modelovanie únavových a medzikryštalických lomov. Vzhľadom k tomu, že tieto lomy nie sú hladké, už kvôli princípu ich pôvodu, sa vymykajú bežným možnostiam matematického opisu. Avšak ak sú splnené podmienky samopodobnosti, umožňujú prostriedky fraktálnej geometrie opísať rôzne nepravidelné, ťažko opísateľné, krivoľaké alebo fragmentované geometrické tvary. Fraktálny opis profilov lomov umožňuje ich presnejšiu kvantifikáciu a identifikáciu možných príčin ich iniciácií. Táto štúdia obsahuje niekoľko príkladov špecifických lomov ocelí Cr-Ni a základné vysvetlenie ich fraktografického opisu. Fractographic methods derive their knowledge from Euclidean geometry, set theory, metric theory and chaos theory. In engineering technology, the fractography is primarily used for modeling of fatigue and intergranular fractures. As such defects are not smooth due the principle of their origin, they cannot be described using ordi-nary mathematical tools. However, if the conditions of self-similarity are met, fractal geometry means can describe various irregular, incomprehensible, crooked or fragmented geometric shapes. Fractographic description of the fracture profile allows more accurate quantification of fractures and it also enables identifying possible causes of their initiation. This study contains several examples of specific cases of Cr-Ni steel failures and a basic explanation of their fractographic description
    Kategória publikačnej činnosti ADM
    Číslo archívnej kópie41445
    Kategória ohlasu JANEKOVÁ, Mariana - KOŠTIALIKOVÁ, Daniela - DUBEC, Andrej - BURGET, Matej - PEŠLOVÁ, Františka. The heat treatment impact on material properties of 34CrNiMo6 steel. In Manufacturing technology. ISSN 1213-2489, 2018, vol. 18, no. 6, pp. 912-916.
    KORČOK, Michal - KOLEDA, Peter - BARCÍK, Štefan - OČKAJOVÁ, Alena - KUČERKA, Martin. Effect of technological and material parameters on final surface quality of machining when milling thermally treated spruce wood. In BioResources. ISSN 1930-2126, 2019, vol. 14, no. 4, pp. 10004-10013.
    PELIT, Huseyin - KORKMAZ, Mustafa - BUDAKÇI, Mehmet. Surface roughness of thermally treated wood cut with different parameters in CNC router machine. In BioResources. ISSN 1930-2126, 2021, vol. 16, no. 3, pp. 5133-5147.
    Katal.org.BB301 - Univerzitná knižnica Univerzity Mateja Bela v Banskej Bystrici
    Báza dátxpca - PUBLIKAČNÁ ČINNOSŤ
    OdkazyPERIODIKÁ-Súborný záznam periodika
    nerozpoznaný

    nerozpoznaný

Počet záznamov: 1  

  Tieto stránky využívajú súbory cookies, ktoré uľahčujú ich prezeranie. Ďalšie informácie o tom ako používame cookies.